PRODUCTS
Contact Us Anytime, We Are Always Here For You
Catalog
Industry
It can be used for automatic submerged arc welding of carbon steel and low alloy steel with equivalent strength level, such as chemical industry, ship, boiler, etc.
JL-WEM12K is compatible with sintered flux JL-SJ101, ensuring stable arc combustion, beautiful weld bead formation, easy slag removal, and high low-temperature impact value of the weld metal.
Requirement for diffusion hydrogen content in deposited metal: ≤ 8.0mL/100g(Mercury Method)
Requirements for S & P Content of Welding Flux :
S ≤ 0.050%2. P ≤ 0.060%
Flux should be baked at 250-400℃ for 1-2 hours before use. Welding wire should be dry, Free of oil and rust before use.
Before welding, impurities such as rust, oil stains, and moisture must be removed from the welded parts.